Polymer Property : Electrical Resistivity = 1.12e+7 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.12e+7 ohm-cm
1.12e+7 ohm-cm
Arkema Group Pebax® 5533 SN 70 NOIR Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion...ISO data provided by the manufacturer, Arkema.