Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 1.00e+6 ohm-cm
1000 - 1.00e+6 ohm-cm
IEC 60093
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon
The integration of 25% carbon increases the wear resistance, hardness, and creep strength of this material. Murflor® + Carbon is used, for example, when electrical conductivity is required and Mate..
Electrical Resistivity 1.00 - 1.00e+6 ohm-cm
1.00 - 1.00e+6 ohm-cm
Average value: 270000 ohm-cm Grade Count:35
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 500000 ohm-cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Electrical Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D257
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 1000 - 1.00e+6 ohm-cm
1000 - 1.00e+6 ohm-cm
ASTM D257
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 117000 ohm-cm Grade Count:15
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Electrical Resistivity 1.00 - 1.00e+6 ohm-cm
1.00 - 1.00e+6 ohm-cm
Average value: 143000 ohm-cm Grade Count:10
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Electrical Resistivity 100 - 1.00e+6 ohm-cm

@Temperature 20.0 °C
100 - 1.00e+6 ohm-cm

@Temperature 68.0 °F
Acerde Silicon Carbide
Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert..
Electrical Resistivity 0.0500 - 1.00e+6 ohm-cm
0.0500 - 1.00e+6 ohm-cm
doped
Mateck Zinc Selenide, ZnSe
Semiconductor single crystals. Twins and stacking faults twin free.