Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 1.00e+18 ohm-cm
1000 - 1.00e+18 ohm-cm
Average value: 2.51e+16 ohm-cm Grade Count:75
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Electrical Resistivity 1000 - 1.00e+18 ohm-cm
1000 - 1.00e+18 ohm-cm
Average value: 1.25e+17 ohm-cm Grade Count:110
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm
1.00e+14 - 1.00e+18 ohm-cm
Average value: 2.90e+17 ohm-cm Grade Count:28
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm
1.00e+14 - 1.00e+18 ohm-cm
Average value: 2.27e+17 ohm-cm Grade Count:9
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm
1.00e+14 - 1.00e+18 ohm-cm
Average value: 1.11e+17 ohm-cm Grade Count:70
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 1.42e+16 ohm-cm Grade Count:81
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Electrical Resistivity 10000 - 1.00e+18 ohm-cm
10000 - 1.00e+18 ohm-cm
Average value: 1.87e+17 ohm-cm Grade Count:44
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Electrical Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
Average value: 8.94e+17 ohm-cm Grade Count:17
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Electrical Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
Average value: 9.55e+17 ohm-cm Grade Count:10
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 7.19e+16 ohm-cm Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 4.11e+16 ohm-cm Grade Count:70
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Electrical Resistivity 1000 - 1.00e+18 ohm-cm
1000 - 1.00e+18 ohm-cm
Average value: 3.64e+16 ohm-cm Grade Count:71
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Electrical Resistivity 1.00e+6 - 1.00e+18 ohm-cm
1.00e+6 - 1.00e+18 ohm-cm
Average value: 3.44e+16 ohm-cm Grade Count:35
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Electrical Resistivity 1.00e+10 - 1.00e+18 ohm-cm
1.00e+10 - 1.00e+18 ohm-cm
Average value: 1.68e+17 ohm-cm Grade Count:6
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm
1.00e+14 - 1.00e+18 ohm-cm
Average value: 1.33e+17 ohm-cm Grade Count:8
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 1.00e+9 - 1.00e+18 ohm-cm
1.00e+9 - 1.00e+18 ohm-cm
Average value: 1.28e+16 ohm-cm Grade Count:96
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Electrical Resistivity 1.00e+13 - 1.00e+18 ohm-cm
1.00e+13 - 1.00e+18 ohm-cm
Average value: 5.20e+16 ohm-cm Grade Count:22
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Electrical Resistivity 1.00e+13 - 1.00e+18 ohm-cm
1.00e+13 - 1.00e+18 ohm-cm
Average value: 6.01e+16 ohm-cm Grade Count:19
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Electrical Resistivity 1000 - 1.00e+18 ohm-cm
1000 - 1.00e+18 ohm-cm
Average value: 2.85e+17 ohm-cm Grade Count:14
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 1.00e+13 - 1.00e+18 ohm-cm
1.00e+13 - 1.00e+18 ohm-cm
Average value: 3.76e+16 ohm-cm Grade Count:33
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved