Polymer Property : Electrical Resistivity = 1.00e+18 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET B-105C PET Bottle Grade
A co-polymer used for soft drinks and other applications.
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET F097H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET F097HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Electrical Resistivity 1e+05 - 1.00e+18 ohm-cm
1e+05 - 1.00e+18 ohm-cm
Average value: 3.51e+16 ohm-cm Grade Count:37
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET B-101C PET Sheet Grade
A sheet grade polymer used in thick films.
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Pearl Engineering PEPLPET B-103C PET Bottle Grade
A co-polymer used for mineral water bottles
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 1e+05 - 1.00e+18 ohm-cm
1e+05 - 1.00e+18 ohm-cm
Average value: 2.70e+17 ohm-cm Grade Count:24
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE)
Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber ..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE)
Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE)
Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low ..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® A.30 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® A.20 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® E2 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® E2 BP PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di..
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..