Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 1.00e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity ..
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co..
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Shell Carilon® DP P1000 Polyketone  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Average value: 1.00e+13 ohm-cm Grade Count:9
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 200C TFE 20  Nylon 11 (PA 11) PTFE 20%  (discontinued **)
PTFE 20%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for thi..
Electrical Resistivity 1.00e+13 - 1.00e+16 ohm-cm
1.00e+13 - 1.00e+16 ohm-cm
Average value: 2.09e+15 ohm-cm Grade Count:16
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
1.00e+13 - 1.00e+14 ohm-cm
Average value: 8.50e+13 ohm-cm Grade Count:6
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 205.3D HS  Nylon 6/12 (PA 6/12) Glass Fiber 33% - Heat Stable  (discontinued
Glass Fiber 33% - Heat StableComments:Glass FiberHeat StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 201D L  Nylon 6/12 (PA 6/12) Glass Fiber 10% - Lubricated  (discontinued **)
Glass Fiber 10% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Electrical Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 93
Solvay Technyl® A 205F Nylon 66, EH50
Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate
Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Propionate 350E0096912 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 13%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
CENTROPLAST CENTROMID 12 Polyamide 12
This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 200 C Z  Nylon 11 (PA 11) FDA Type  (discontinued **)
FDA TypeComments:FDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this ..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 205D  Nylon 6/12 (PA 6/12) Glass Fiber 30%  (discontinued **)
Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
RTP Company RTP 207D FR  Nylon 6/12 (PA 6/12) Glass Fiber 40% - Flame Retardant  (discontinu
Glass Fiber 40% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Electrical Resistivity 1.00e+13 - 2.00e+20 ohm-cm
1.00e+13 - 2.00e+20 ohm-cm
Average value: 1.03e+19 ohm-cm Grade Count:37
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..