Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
Special Metals MONEL® Alloy R-405 The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Heavily Cold Rolled Sheet and Strip, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Electrical Resistivity | 0.0000510 ohm-cm | 0.0000510 ohm-cm | |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Annealed Plate, Sheet, and Strip, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |