Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Nihon Superior SN100C Lead-Free Solder Alloy Allows high productivity in soldering processes and cost effective, reliable joints. Attributes include high fluidity, low copper erosion, low drossing, superior wetting and freedom from shrinkage d.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Hogen HM1150 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Hogen HM3050 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Mi-Tech Metals HD17.5 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Mi-Tech Metals HD18D Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
Indium Corp. Indalloy® 2 In-Pb-Ag Solder Alloy Especially useful for soldering against gold, as leaching is minimized. Good thermal fatigue properties. Compatible with Indalloy numbers 204, 205, 206, 7, 10 and 150 in step-soldering applications... |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Electrical Resistivity | 0.0000130 ohm-cm | 0.0000130 ohm-cm | |
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |