Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.00000636 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, 1/2 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, 1/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, 3/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, Annealed
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, Extra Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, Extra Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 260 Cartridge Brass, Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, 1/2 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, 1/4 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, 3/4 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, Annealed
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, Extra Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, Extra Spring
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Eagle Brass 425 Tin Brass 2%, Spring
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Copyright © lookpolymers.com All Rights Reserved