Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000004914 ohm-cm | 0.000004914 ohm-cm | |
ALIMEX ACP 5080 Aluminum Cast Plate ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum.. |
|||
Electrical Resistivity | 0.000004914 ohm-cm | 0.000004914 ohm-cm | |
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |