Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Annealed Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ AT Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
(55% IACS Conductivity)
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Electrical Resistivity 0.00000310 ohm-cm
0.00000310 ohm-cm
55 % IACS
CMW® ELKONITE 40SB tungsten, silver