Electrical Properties Metric English Comments
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, 1/2 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, 1/4 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, 3/4 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, Annealed
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, Extra Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, Extra Spring
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 110 EPT COPPER, Spring
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), 3/4 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), Annealed
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), Extra Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), Extra Spring
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), Spring
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), 1/4 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), 3/4 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Annealed
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Extra Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 102 OF COPPER (Non-Certified), Spring
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed
Eagle Brass 101 OFE COPPER (Certified), 1/4 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Electrical Resistivity <= 0.00000176 ohm-cm
<= 0.00000176 ohm-cm
Calculated from Min 98 %IACS
Cadi C10100 Oxygen Free Copper
Oxygen Free Copper is specified when resistance to hydrogen embrittlement is required due to application in a high temperature, hydrogen environment.Forms: RodBarPlateInformation provided by Cadi Co..
Electrical Resistivity <= 0.00000176 ohm-cm
<= 0.00000176 ohm-cm
Calculated from Min 98 %IACS
Cadi C11000 ETP Standard Grade Copper
The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern...