Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 3.00 mm |
>= 300 sec @Thickness 0.118 in |
PLC 0; UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 0.750 mm |
>= 300 sec @Thickness 0.0295 in |
NC |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 3.00 mm |
>= 300 sec @Thickness 0.118 in |
BK, BN |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 0.840 mm |
>= 300 sec @Thickness 0.0331 in |
BK |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 1.50 mm |
>= 300 sec @Thickness 0.0591 in |
BK |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec | >= 300 sec | UL 746 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec | >= 300 sec | UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 1.50 mm |
>= 300 sec @Thickness 0.0591 in |
BK |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec | >= 300 sec | UL 746 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec @Thickness 0.750 mm |
>= 300 sec @Thickness 0.0295 in |
BK |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
High Voltage Arc Resistance to Ignition (HVAR) | >= 300 sec | >= 300 sec | PLC 0; UL 746 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |