Polymer Property : High Amp Arc Ignition, HAI = 0.00 arcs Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 0.00 - 15 arcs

@Thickness 0.710 mm
0.00 - 15 arcs

@Thickness 0.0280 in
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
High Amp Arc Ignition, HAI 0.00 - 15 arcs

@Thickness 0.710 mm
0.00 - 15 arcs

@Thickness 0.0280 in
LG Chemical Lupox® GP2076F PBT+GF7%
Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical