Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.800 mm |
7.0 - 15 sec @Thickness 0.0315 in |
UL 746 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.550 mm |
7.0 - 15 sec @Thickness >=0.0217 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.80 mm |
7.0 - 15 sec @Thickness >=0.0709 in |
|
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
All colors |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746A |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |