Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 120 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
UL 746
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 0.750 mm
>= 120 sec

@Thickness 0.0295 in
UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 0.750 mm
>= 120 sec

@Thickness 0.0295 in
PLC 0; UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0; UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
PLC 0; UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
NC
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
BK, BN
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
BN, BK
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 0.800 mm
>= 120 sec

@Thickness 0.0315 in
PLC 0
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.60 mm
>= 120 sec

@Thickness 0.0630 in
All colors; PLC 0
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 2.00 mm
>= 120 sec

@Thickness 0.0787 in
All colors; PLC 0
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
All colors; PLC 0
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
NC; PLC 0
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 0.800 mm
>= 120 sec

@Thickness 0.0315 in
PLC 0
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded
Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
PLC 0
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded
Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
PLC 0
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded
Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
PLC 0
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 0.750 mm
>= 120 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
(BK)
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
UL 746A
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..