Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 371 - 410 °C | 700 - 770 °F | Molding |
PolyOne Stat-Tech™ PI-30GF/15SS Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Electrically ConductiveGlass Fiber ReinforcedStainless Steel Fiber FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |
|||
Melt Temperature | 371 - 410 °C | 700 - 770 °F | Molding |
PolyOne Edgetek® PI-30CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 371 - 410 °C | 700 - 770 °F | Molding |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 300 - 410 °C | 572 - 770 °F | Average value: 356 °C Grade Count:9 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Melt Temperature | 271 - 410 °C | 520 - 770 °F | Average value: 352 °C Grade Count:9 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |