Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 302 - 350 °C | 575 - 662 °F | Average value: 327 °C Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 320 - 350 °C | 608 - 662 °F | |
LATI LAPEX A Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 325 - 350 °C | 617 - 662 °F | |
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 325 - 350 °C | 617 - 662 °F | |
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 330 - 350 °C | 626 - 662 °F | |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Melt Temperature | 330 - 350 °C | 626 - 662 °F | |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Melt Temperature | 330 - 350 °C | 626 - 662 °F | |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Melt Temperature | 340 - 350 °C | 644 - 662 °F | |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Melt Temperature | 300 - 350 °C | 572 - 662 °F | |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Melt Temperature | 302 - 350 °C | 575 - 662 °F | Average value: 326 °C Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Temperature | 302 - 350 °C | 575 - 662 °F | Average value: 327 °C Grade Count:18 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Melt Temperature | 340 - 350 °C | 644 - 662 °F | |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |