Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | |
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C230GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Melt Temperature | 350 - 390 °C | 662 - 734 °F | Injection molding/extrusion |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Melt Temperature | 350 °C | 662 °F | Optimal |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 350 - 370 °C | 662 - 698 °F | |
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Melt Temperature | 350 - 370 °C | 662 - 698 °F | |
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |