Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 349 - 371 °C | 660 - 700 °F | |
Oxford Polymers PEI 30GF-Natural PEI, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristic.. |
|||
Melt Temperature | 349 - 400 °C | 660 - 752 °F | Average value: 376 °C Grade Count:9 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Melt Temperature | 349 - 377 °C | 660 - 711 °F | injection molding |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Melt Temperature | 349 - 388 °C | 660 - 730 °F | Molding |
PolyOne Lubri-Tech™ RA-15GF/13T Polyethersulfone, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |