Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 345 - 385 °C | 653 - 725 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Melt Temperature | 345 - 390 °C | 653 - 734 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Melt Temperature | 345 - 385 °C | 653 - 725 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Melt Temperature | 345 - 385 °C | 653 - 725 °F | |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Melt Temperature | 345 - 385 °C | 653 - 725 °F | |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |