Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 338 - 427 °C | 640 - 800 °F | |
Oxford Polymers PEI 1000 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Temperature | 338 - 371 °C | 640 - 700 °F | |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 338 - 427 °C | 640 - 800 °F | |
Oxford Polymers PEI 1010 PEI Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: .. |
|||
Melt Temperature | 338 - 371 °C | 640 - 700 °F | Stock |
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Molding |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Stock |
PolyOne Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Molding |
PolyOne Edgetek® PF-1000 Polysulfone
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |