Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 330 - 352 °C | 626 - 666 °F | Injection |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Melt Temperature | 330 - 360 °C | 626 - 680 °F | |
LATI LAPEX A G/30 30% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding |
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding |
Covestro Apec® DP 1-9349/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding |
Covestro Apec® DP 1-9359/7 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding |
Covestro Apec® DP 1-9379/7 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M.. |
|||
Melt Temperature | 330 °C | 626 °F | Resin, Injection Molding |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Melt Temperature | 330 - 345 °C | 626 - 653 °F | |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection molding; ISO 294 |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding; ISO 294 |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding; ISO 294 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding; ISO 294 |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Melt Temperature | 330 - 340 °C | 626 - 644 °F | |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Melt Temperature | 330 °C | 626 °F | Injection Molding; ISO 294 |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Melt Temperature | 330 °C | 626 °F | Injection molding; ISO 294 |
Covestro Apec® FR1892 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |