Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 221 - 238 °C | 430 - 460 °F | Molding |
PolyOne Edgetek® AS-10CF/000 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 °C | 430 °F | |
Chevron Phillips HiD® 9632 HDPE Blown Film Resin
(discontinued **) Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre.. |
|||
Melt Temperature | 221 - 249 °C | 430 - 480 °F | Molding |
PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 °C | 430 °F | Molding |
PolyOne Stat-Tech™ AS-08CF/000 Black Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(disconti Description/Features:Carbon Fiber ReinforcedESD ProtectionPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | Average value: 249 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 221 °C | 430 °F | |
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma.. |
|||
Melt Temperature | <= 221 °C | <= 430 °F | |
LyondellBasell Ultrathene® UE637000 Ethylene Vinyl Acetate Copolymer, Film Extrusion Grade ULTRATHENE UE637000 is an EVA copolymer with good toughness, flexibility and clarity. Applications include laminating and heavy duty films as well as injection and blow molding. UE637000 contains no.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 221 - 260 °C | 430 - 500 °F | |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 221 °C | 430 °F | |
LyondellBasell Petrothene® NA362005 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
Melt Temperature | 221 °C | 430 °F | |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Melt Temperature | 221 - 229 °C | 430 - 445 °F | Processing Temperature |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Melt Temperature | 221 °C | 430 °F | |
E-Polymers SEPAZ® N1040 Nanoclay 4% High Flow Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Melt Temperature | 221 °C | 430 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B901 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 221 °C | 430 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |