Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 415 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 213 - 216 °C
415 - 421 °F
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
LyondellBasell Petrothene® LP540200 High Density Polyethylene
ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 213 °C
415 °F
Injection Molding
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Melt Temperature 213 °C
415 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Copyright © lookpolymers.com All Rights Reserved