Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 393 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 360 - 393 °C
680 - 739 °F
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU)
Information provided by PolyOne
Melt Temperature 382 - 393 °C
720 - 740 °F
Molding
PolyOne Edgetek® PK-20GF/000 Polyetheretherketone (PEEK), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved