Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 349 - 377 °C | 660 - 711 °F | injection molding |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber Data provided by Clariant Masterbatches |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP003 Polyetheretherketone, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 349 - 388 °C | 660 - 730 °F | Molding |
PolyOne Lubri-Tech™ RA-15GF/13T Polyethersulfone, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |