Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | Injection Molding |
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | |
LG Chemical LUPOY GP-2301F General Purpose Modified PC, 30% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | <= 300 °C | <= 572 °F | Processing Temperature |
Teknor Apex Beetle® MD82 Nylon 6, Non-halogenated, Dry Notes: MD82 is a UL recognized, V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 6; U.L. 94 V-O at 0.63mm. Colorable Features: Fla.. |
|||
Melt Temperature | <= 300 °C | <= 572 °F | Processing Temperature |
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F.. |
|||
Melt Temperature | <= 300 °C | <= 572 °F | Processing Temperature |
Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced Notes: MDM54 is a UL recognized, V-2 rated halogen and phosphorus-free flam retarded, mineral filled injection molding grade of nylon 6, primarily intended for electrical applications; U.L. 94 V-2 a.. |
|||
Melt Temperature | 300 - 310 °C | 572 - 590 °F | |
Samyang Trirex® 3030IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding |
Covestro Makrolon® 3158 Polycarbonate Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® Rx1805 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V200L Unfilled PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o.. |
|||
Melt Temperature | 300 °C | 572 °F | Optimal |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® K365GM 60% Glass Fiber/Calcium Carbonate Reinforced General Purpose PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Melt Temperature | 300 - 410 °C | 572 - 770 °F | Average value: 356 °C Grade Count:9 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |