Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 241 - 291 °C | 466 - 556 °F | Injection |
Albis Plastics Polyamide 6/66 PA 152 GF30/02 BK8-1114 Black 30% Glass Fiber
(discontinued **) Semi-crystalline Nylon 6/66 (PA6/66)Characteristics: Industrial GradeApplications: Office Furniture, Gear, Housings and ConnectorsProcessing: Injection Molding (Melt Temperature: 465 -555°F, Mold .. |
|||
Melt Temperature | 220 - 291 °C | 428 - 556 °F | Average value: 260 °C Grade Count:47 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |