Processing Properties Metric English Comments
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Wire & Cable EMB405LB Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Wire & Cable W1349L NAT 0000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx09FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Wire & Cable W2403 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid)
All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne
Melt Temperature 179 - 191 °C
354 - 376 °F
PolyOne Geon™ Vinyl Flexible A48248D Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 179 - 191 °C
354 - 376 °F
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Flexible R132BE Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Flexible R157AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 179 - 191 °C
354 - 376 °F
PolyOne Geon™ Vinyl Flexible R1700E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 179 - 191 °C
354 - 376 °F
PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Flexible XV3881 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Flexible F78E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Flexible R4294U Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Flexible R4294W Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 177 - 191 °C
350 - 375 °F
Extrusion
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE
Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri..
Melt Temperature 177 - 191 °C
350 - 375 °F
Sylvin Technologies 9077-75C Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Melt Temperature 177 - 191 °C
350 - 375 °F
Sylvin Technologies 9604-80C Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Melt Temperature 177 - 191 °C
350 - 375 °F
Sylvin Technologies 9604-85C Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Melt Temperature 185 - 191 °C
365 - 376 °F
PolyOne Geon™ Vinyl Flexible R339AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 177 - 191 °C
351 - 376 °F
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 177 - 191 °C
350 - 375 °F
Sylvin Technologies 9604-95C Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Melt Temperature 182 - 191 °C
360 - 376 °F
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..