Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1100 - 1260 °C | 2010 - 2300 °F | |
Wieland Simidur KF Plus PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |