Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 8640 - 11520 min @Temperature 20.0 °C |
8640 - 11520 min @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Pot Life | 8640 - 10080 min @Temperature 20.0 °C |
8640 - 10080 min @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |