Polymer Property : Pot Life = 480 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 480 min

@Temperature 25.0 °C
480 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) FR-1200 / EA-117 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 480 min

@Temperature 25.0 °C
480 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) FR-1210 / EA-117 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 480 min

@Temperature 25.0 °C
480 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) FR-1610 / EA-039 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-21 High-Performance Dielectric Epoxy
AboCast 8103-21 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines r..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-24 High-Performance Dielectric Epoxy
AboCast 8103-24 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has an exc..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-26 High-Performance Dielectric Epoxy
AboCast 8103-26 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-27 High-Performance Dielectric Epoxy
AboCast 8103-27 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-28 High-Performance Dielectric Epoxy
AboCast 8103-28 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-20 High-Performance Dielectric Epoxy
AboCast 8103-20 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is unique ..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy
AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-25 High-Performance Dielectric Epoxy
AboCast 8103-25 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines o..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-29 High-Performance Dielectric Epoxy
AboCast 8103-29 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-30 High-Performance Dielectric Epoxy
AboCast 8103-30 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h..
Pot Life 480 min

@Temperature 24.0 °C
480 min

@Temperature 75.2 °F
Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating
Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating f..
Pot Life 480 min

@Temperature 23.9 °C
480 min

@Temperature 75.0 °F
Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating
Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating f..
Pot Life >= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Abatron AboCast 8103-22 High-Performance Dielectric Epoxy
AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in..