Polymer Property : Pot Life = 15 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 11 - 15 min

@Temperature 24.0 °C
11 - 15 min

@Temperature 75.2 °F
A/C
Lord Adhesives 7542 Urethane Adhesive
LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L..
Pot Life 10 - 15 min

@Temperature 40.0 °C
10 - 15 min

@Temperature 104 °F
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive
LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo..