Polymer Property : Shelf Life = 3.00 Month Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 12K GA090 Uni Tape Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 3K 8HS PAN Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7628 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, Silica Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced
Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced
Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..