Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 1.00 - 2.00 min | 1.00 - 2.00 min | |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Gel Time | 1.00 - 2.00 min | 1.00 - 2.00 min | |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Gel Time | 1.10 - 2.00 min @Temperature 124 °C |
1.10 - 2.00 min @Temperature 255 °F |
|
Park Electrochemical Nelcote® P-601 Polyester Prepreg, 18oz. Woven Fiberglass Roving P-601 Polyester is a fire retardant prepreg resin system, which meets the requirements of MIL-R-7575. P-601 prepregs are available on any style of woven fiberglass fabric having a suitable finish, s.. |