Polymer Property : Gel Time = 2.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 1.00 - 2.00 min
1.00 - 2.00 min
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Gel Time 1.00 - 2.00 min
1.00 - 2.00 min
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Gel Time 1.10 - 2.00 min

@Temperature 124 °C
1.10 - 2.00 min

@Temperature 255 °F
Park Electrochemical Nelcote® P-601 Polyester Prepreg, 18oz. Woven Fiberglass Roving
P-601 Polyester is a fire retardant prepreg resin system, which meets the requirements of MIL-R-7575. P-601 prepregs are available on any style of woven fiberglass fabric having a suitable finish, s..