Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gel Time = 0.167 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 0.167 - 0.333 min
0.167 - 0.333 min
400 watt UV
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System
Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas..
Gel Time 0.167 - 0.200 min
0.167 - 0.200 min
Dow SPECTRIM™ MM310 Reaction Moldable Polymer
SPECTRIM™ MM 310 reaction moldable polymer is a three-component, fast-reacting, low viscosity polycarbamate system ideally suited for mat molding of structural composites. The structural reaction ..
Copyright © lookpolymers.com All Rights Reserved