Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |