Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1201-15 Polyester SMC Premi-Glas® 1201-15 is a 15% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC QC-8700 is a vinyl ester engineered structural composite molding compound for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested f.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |