Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC QC-8700 is a vinyl ester engineered structural composite molding compound for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested f.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |