Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Annealing Temperature = 830.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 830.0 - 860 °C
1526 - 1580 °F
Soft; Cooling: Furnace; < 250HB
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel
Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools ..