Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Roll Temperature | 90.0 °C | 194 °F | 1st |
Kostat E-3007J Conductive PS Compound KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea.. |