Processing Properties Metric English Comments
Roll Temperature 75.0 - 95.0 °C
167 - 203 °F
Average value: 85.0 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Roll Temperature 75.0 - 85.0 °C
167 - 185 °F
Bottom
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Roll Temperature 75.0 - 85.0 °C
167 - 185 °F
Bottom
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Roll Temperature 75.0 - 85.0 °C
167 - 185 °F
Bottom
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Roll Temperature 75.0 - 85.0 °C
167 - 185 °F
Bottom
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Roll Temperature 75.0 - 85.0 °C
167 - 185 °F
Bottom
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..