Processing Properties Metric English Comments
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 45.0 - 55.0 °C
113 - 131 °F
Temperature of Engraved Rolls
EMS-Griltech Griltex® D 1712A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..