Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 90.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 60.0 - 90.0 min
1.00 - 1.50 hour
handling time
Permabond ET536 Epoxy Resin
PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo..
Cure Time 60.0 - 90.0 min

@Temperature 149 - 177 °C
1.00 - 1.50 hour

@Temperature 300 - 350 °F
Master Bond EP13 High Temperature Resistant One Component Epoxy System
Master Bond Polymer System EP13 is a one component heat curing epoxy featuring high shear strength and very high temperature resistance. EP13 forms rigid and dimensionally stable bonds with minimal ..
Cure Time 60.0 - 90.0 min

@Temperature 149 - 177 °C
1.00 - 1.50 hour

@Temperature 300 - 350 °F
Master Bond EP15 High Tensile Strength One Component Epoxy
Master Bond Polymer System EP15 is a one component, heat curing epoxy featuring high tensile strength utilized in testing the adhesion and/or cohesive strength of flame-sprayed coatings. This standa..
Cure Time 45.0 - 90.0 min

@Temperature 22.0 °C
0.750 - 1.50 hour

@Temperature 71.6 °F
Dow Corning 3-4150 DIELECTRIC GEL KIT
Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning
Cure Time 30.0 - 90.0 min

@Temperature 100 - 160 °C
0.500 - 1.50 hour

@Temperature 212 - 320 °F
or longer
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating
AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve..
Cure Time 60.0 - 90.0 min
1.00 - 1.50 hour
Hard Dry
3M Scotchkote™ XF 895 Fast Curing Floor Coating
Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to serviceProduct Fe..
Cure Time 60.0 - 90.0 min
1.00 - 1.50 hour
Tack-Free, 50% RH
3M 540 Polyurethane Sealant
3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The..
Cure Time 50.0 - 90.0 min
0.833 - 1.50 hour
Tack-Free, 50% RH
3M 550 Polyurethane Adhesive Sealant Fast Cure
3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The..
Copyright © lookpolymers.com All Rights Reserved