Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 9.50 min @Temperature 68.3 °C |
0.158 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 9.50 min @Temperature 68.3 °C |
0.158 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 9.50 min @Temperature 68.3 °C |
0.158 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 9.50 min | 0.158 hour | t`90, Target; ASTM D2084 |
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical |
|||
Cure Time | 9.50 min | 0.158 hour | Curelastmeter |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Cure Time | 9.50 min @Temperature 68.3 °C |
0.158 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |