Polymer Property : Cure Time = 7.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 5.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Cure Time 7.00 min

@Temperature 83.3 °C
0.117 hour

@Temperature 182 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 83.3 °C
0.117 hour

@Temperature 182 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min
0.117 hour
Loctite® 246 High Temperature/Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min
0.117 hour
t`50, Target; ASTM D2084
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical
Cure Time 7.00 min
0.117 hour
t`50, Target; ASTM D2084
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Cure Time 7.00 min

@Temperature 83.3 °C
0.117 hour

@Temperature 182 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 83.3 °C
0.117 hour

@Temperature 182 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 160 °C
0.117 hour

@Temperature 320 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 5.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 149 °C
0.117 hour

@Temperature 300 °F
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
Cure Time 7.00 min

@Temperature 160 °C
0.117 hour

@Temperature 320 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 7.00 - 10.0 min

@Temperature 25.0 °C
0.117 - 0.167 hour

@Temperature 77.0 °F
demold time
BCC Products BC 8086 Urethane Casting
BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: no..