Polymer Property : Cure Time = 504 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 10100 - 30200 min

@Temperature 24.0 °C
168 - 504 hour

@Temperature 75.2 °F
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure..
Cure Time 5.00 - 30200 min
0.0833 - 504 hour
Average value: 2920 min Grade Count:19
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Cure Time 1.00 - 30200 min
0.0167 - 504 hour
Average value: 3380 min Grade Count:18
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..