Processing Properties Metric English Comments
Cure Time 4.90 min

@Temperature 177 °C
0.0817 hour

@Temperature 350 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 4.90 min

@Temperature 177 °C
0.0817 hour

@Temperature 350 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 4.90 min

@Temperature 177 °C
0.0817 hour

@Temperature 350 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 4.90 min

@Temperature 177 °C
0.0817 hour

@Temperature 350 °F
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..