Processing Properties Metric English Comments
Cure Time 30.0 - 35.0 min
0.500 - 0.583 hour
fixture timee
Permabond TA4820 Structural Acrylic Adhesive
PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites.  TA4820 has excellent adhesion to as received metal surfac..
Cure Time 30.0 - 35.0 min
0.500 - 0.583 hour
Fixture time
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White
Information provided by ITW Devcon
Cure Time 30.0 - 35.0 min
0.500 - 0.583 hour
Fixture time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black